Description
Truly excellent corrosion resistance can be obtained when Cr2O3-25TiO2 powder is applied over a corrosion resistant bond coat, such as nickel chromium, and subsequently sealed.
Service Temperature: ≤ 540 °C (1000 °F)
Chemical Composition
| Cr2O3 | TiO2 | SiO2 | Fe2O3 |
| Bal. | 23.0 – 27.0 | < 0.2 | < 0.2 |
Application
- Resistance to abrasive grains at low temperatures in applications such as mandrels for dry cell battery cores and oil industry sucker rod couplings
- Resistant to hard surfaces at low temperatures in applications such as drum doctor blades and machine tool chip breakers



Reviews
There are no reviews yet.